VARIDUR 200 KIT
Click SDS for details

Item No: 111039
VariDur 200 is a blue, mineral filled acrylic for good edge retention with a 8 min cure time.
VariDur 200 is a blue, mineral filled acrylic for good edge retention with a 8 min cure time.
Products specifications
PRODUCT FAMILY VariDur 200
QTY/EA 1
TYPE Kit
Products specifications
PRODUCT FAMILY VariDur 200
QTY/EA 1
TYPE Kit