ULTRAPOL, PSA, 10 IN
Item No: 407450
UltraPol is a hard, woven, non-aggressive silk cloth. It is used to maintain excellent flatness during intermediate polishing especially for mixed materials. The non-aggressive material removal rate minimizes surface damage. Typical applications include but are not limited to minerals, coals, inclusion retention in steels and refractory metals.
UltraPol is a hard, woven, non-aggressive silk cloth. It is used to maintain excellent flatness during intermediate polishing especially for mixed materials. The non-aggressive material removal rate minimizes surface damage. Typical applications include but are not limited to minerals, coals, inclusion retention in steels and refractory metals.
Products specifications
BACKING PSA Backed
DIMENSIONS 10 in [254 mm]
PRODUCT FAMILY UltraPol
QTY/EA 10