PhenoCure PreMolds, Black, 1in

PHENOCURE PREMOLDS, BLACK, 1IN
Click SDS for details

Item No: 203111501
PhenoCure PreMolds are a phenolic thermoset resin that provide good edge retention with moderate shrinkage for general metallurgy. Premolds can reduce mess and save time compared to PhenoCure powder. They are available in Black, Red, or Green colors.
PhenoCure PreMolds are a phenolic thermoset resin that provide good edge retention with moderate shrinkage for general metallurgy. Premolds can reduce mess and save time compared to PhenoCure powder. They are available in Black, Red, or Green colors.