MicroPolish II Suspension, 0.3µm, 1 gal

MICROPOLISH II SUSPENSION, 0.3?M, 1 GAL
Click SDS for details

Item No: 406363128

MicroPolish II powders contain high quality deagglomerated alumina oxide particules for final polishing. They provide better surface finishes than agglomerated versions and a suitable for most minerals and metals.

MicroPolish II powders contain high quality deagglomerated alumina oxide particules for final polishing. They provide better surface finishes than agglomerated versions and a suitable for most minerals and metals.

Products specifications
ABRASIVE MATERIAL Alumina
CONTAINER SIZE 1 gal [3.8 L]
MICRON SIZE 0.3 µm
PRODUCT FAMILY MicroPolish II
QTY/EA 1
TYPE Suspension
Products specifications
ABRASIVE MATERIAL Alumina
CONTAINER SIZE 1 gal [3.8 L]
MICRON SIZE 0.3 µm
PRODUCT FAMILY MicroPolish II
QTY/EA 1