MICROCUT PSA, 800 [P1500], 8IN
Item No: 36080800
MicroCut S offers a fine grit silicon carbide paper providing gentle material removal and excellent surface finish. They contain a PSA backing for application directly to the platen or a magnetic carrier plate.
MicroCut S offers a fine grit silicon carbide paper providing gentle material removal and excellent surface finish. They contain a PSA backing for application directly to the platen or a magnetic carrier plate.
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 8 in [203 mm]
GRIT SIZE 800 [P1500]
PRODUCT FAMILY MicroCut
QTY/EA 100
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 8 in [203 mm]
GRIT SIZE 800 [P1500]
PRODUCT FAMILY MicroCut