Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 8 in [203 mm]
GRIT SIZE 1200 [P2500]
PRODUCT FAMILY MicroCut
QTY/EA 100
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 8 in [203 mm]
GRIT SIZE 1200 [P2500]
PRODUCT FAMILY MicroCut