MICROCUT PSA, 800 [P1500], 10IN
Item No: 36100800
MicroCut S offers a fine grit silicon carbide paper providing gentle material removal and excellent surface finish. They contain a PSA backing for application directly to the platen or a magnetic carrier plate.
MicroCut S offers a fine grit silicon carbide paper providing gentle material removal and excellent surface finish. They contain a PSA backing for application directly to the platen or a magnetic carrier plate.
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 10 in [254 mm]
GRIT SIZE 800 [P1500]
PRODUCT FAMILY MicroCut