MICROCUT PSA, 1200 [P2500], 10IN
Item No: 36101200
MicroCut S offers a fine grit silicon carbide paper providing gentle material removal and excellent surface finish. They contain a PSA backing for application directly to the platen or a magnetic carrier plate.
MicroCut S offers a fine grit silicon carbide paper providing gentle material removal and excellent surface finish. They contain a PSA backing for application directly to the platen or a magnetic carrier plate.
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 10 in [254 mm]
GRIT SIZE 1200 [P2500]
PRODUCT FAMILY MicroCut
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 10 in [254 mm]
GRIT SIZE 1200 [P2500]
PRODUCT FAMILY MicroCut