MASTERPREP SUSPENSION, 64OZ
Click SDS for details

Item No: 406377064

MasterPrep is a 0.06µm sol-gel alumina suspension. It is excellent for minerals, ferrous metals, low melting point alloys, carbides, PWBs, precious metals and electronics.

MasterPrep is a 0.06µm sol-gel alumina suspension. It is excellent for minerals, ferrous metals, low melting point alloys, carbides, PWBs, precious metals and electronics.

Products specifications
ABRASIVE MATERIAL Alumina
CONTAINER SIZE 64 oz [1.9 L]
MICRON SIZE 0.05 µm
PRODUCT FAMILY MasterPrep
QTY/EA 1
TYPE Suspension