MasterPolish Alumina & Silica Suspension, 32oz

MASTERPOLISH SUSPENSION, 32OZ
Click SDS for details

Item No: 4010084

Masterpolish final polishing suspensions contain a blend of 0.05µm high purity alumina and colloidal silica with 9pH. It is excellent for use with magnesium alloys, cobalt alloys, most iron alloys, nickel, and metal matrix composites.

Masterpolish final polishing suspensions contain a blend of 0.05µm high purity alumina and colloidal silica with 9pH. It is excellent for use with magnesium alloys, cobalt alloys, most iron alloys, nickel, and metal matrix composites.

Products specifications
ABRASIVE MATERIAL Alumina & Silica
CONTAINER SIZE 32 oz [0.95 L]
MICRON SIZE 0.05 µm
PRODUCT FAMILY MasterPolish
QTY/EA 1
TYPE Suspension
Products specifications
ABRASIVE MATERIAL Alumina & Silica
CONTAINER SIZE 32 oz [0.95 L]
MICRON SIZE 0.05 µm
PRODUCT FAMILY MasterPolish
QTY/EA 1
TYPE Suspension