CARBIMET S, 180 [P180], 8IN
Item No: 16080180
CarbiMet S is a specialized silicon carbide grinding paper that provide rapid material removal and uniform surface finish. They utilize a backing compatible with the Apex S carrier film for fast removal from the platen.
CarbiMet S is a specialized silicon carbide grinding paper that provide rapid material removal and uniform surface finish. They utilize a backing compatible with the Apex S carrier film for fast removal from the platen.
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING Apex S Backed
DIMENSIONS 8 in [203 mm]
GRIT SIZE 180 [P180]
PRODUCT FAMILY CarbiMet
QTY/EA 100
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING Apex S Backed
DIMENSIONS 8 in [203 mm]
GRIT SIZE 180 [P180]
PRODUCT FAMILY CarbiMet