*CARBIMET PSA, 180 [P180], 12IN
Item No: 36120180
CarbiMet is a specialized silicon carbide grinding paper that provide rapid material removal and uniform surface finish. They contain a PSA backing for application directly to the platen or a magnetic carrier plate.
CarbiMet is a specialized silicon carbide grinding paper that provide rapid material removal and uniform surface finish. They contain a PSA backing for application directly to the platen or a magnetic carrier plate.
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 12 in [305 mm]
GRIT SIZE 180 [P180]
PRODUCT FAMILY CarbiMet
Products specifications
ABRASIVE MATERIAL Silicon Carbide
BACKING PSA Backed
DIMENSIONS 12 in [305 mm]
GRIT SIZE 180 [P180]
PRODUCT FAMILY CarbiMet