Products specifications
ABRASIVE MATERIAL Diamond
BACKING Metal Backed
COLOR Black
DIMENSIONS 12 in [305 mm]
MICRON SIZE 125 µm
PRODUCT FAMILY Apex DGD Color
QTY/EA 1
Products specifications
ABRASIVE MATERIAL Diamond
BACKING Metal Backed
COLOR Black
DIMENSIONS 12 in [305 mm]
MICRON SIZE 125 µm
PRODUCT FAMILY Apex DGD Color