AcuThin Blade, >HRC45, 12in [305mm]

ACUTHIN BLADE, >HRC45, 12IN [305MM]
Item No: 103002
The AcuThin series offers thin blades that have been developed to minimize the area of cutting thus reducing the amount of damage to the sample. These blades allow for precise, delicate abrasive sectioning with minimal surface damage.
The AcuThin series offers thin blades that have been developed to minimize the area of cutting thus reducing the amount of damage to the sample. These blades allow for precise, delicate abrasive sectioning with minimal surface damage.
Products specifications
ARBOR SIZE 1.25 in [31.75 mm]
BLADE THICKNESS 0.063 in [1.6 mm]
DIMENSIONS 12 in [305 mm]
PRODUCT FAMILY AcuThin
QTY/EA 10
Products specifications
ARBOR SIZE 1.25 in [31.75 mm]
BLADE THICKNESS 0.063 in [1.6 mm]
DIMENSIONS 12 in [305 mm]
PRODUCT FAMILY AcuThin
QTY/EA 10