775HV0.5 VICKERS TEST BLOCK
Item No: 93005775

Micro-Vickers Test Block calibrated in accordance with ASTM E92 & ISO 6507. Nominal hardness range for standard test blocks is +/- 25HV.

Micro-Vickers Test Block calibrated in accordance with ASTM E92 & ISO 6507. Nominal hardness range for standard test blocks is +/- 25HV.

Products specifications
HARDNESS SCALE HV0.5
HARDNESS VALUE 775HV0.5
PRODUCT FAMILY Vickers