515HV10 VICKERS TEST BLOCK
Item No: 93100515

Macro-Vickers Test Block calibrated in accordance with ASTM E92 & ISO 6507. Nominal hardness range for standard test blocks is +/- 25HV.

Macro-Vickers Test Block calibrated in accordance with ASTM E92 & ISO 6507. Nominal hardness range for standard test blocks is +/- 25HV.

Products specifications
HARDNESS SCALE HV10
HARDNESS VALUE 515HV10
PRODUCT FAMILY Vickers
Products specifications
HARDNESS SCALE HV10
HARDNESS VALUE 515HV10
PRODUCT FAMILY Vickers