450HV1 VICKERS TEST BLOCK
Item No: 93010450

Macro-Vickers Test Block calibrated in accordance with ASTM E92 & ISO 6507. Nominal hardness range for standard test blocks is +/- 25HV.

Macro-Vickers Test Block calibrated in accordance with ASTM E92 & ISO 6507. Nominal hardness range for standard test blocks is +/- 25HV.

Products specifications
HARDNESS SCALE HV1
HARDNESS VALUE 450HV1
PRODUCT FAMILY Vickers